In addition, slag viscosity decreases with increasing smelting time. The experimental results show that extending the smelting time increases the FeO content in the slag, the LV rose from 0.66 to 5.02, the LTi declined from 206.90 to 114.86, the shorter smelting time is favorable for increasing the recovery ratio of vanadium and titanium in metal and slag. The relationship between slag viscosity and temperature at different smelting times was further revealed by thermodynamic calculations. In this work, the effect of smelting time on the distribution behavior and recovery rates of vanadium and titanium in HIsmelt smelting of vanadium–titanium magnetite was investigated by experiment for the first time. HIsmelt is well suited for smelting vanadium–titanium magnetite due to its flexibility in feedstock selection and tolerance to high viscosity slag, compared with the blast furnace.